Low Temperature Silver Brazing Alloys ( Cadmium Bearing )

Low Temperature Silver Brazing Alloys - Cadmium Bearing

Maheshwari Brazings Pvt. Ltd., lowest temperature with short melting ranges, free flowing alloys that are versatile, easy to use having high strength. This family of brazing alloy like high silver brazing alloys has excellent flow characteristics and mechanical properties. Being used successfully for the last many decades on nearly all ferrous and non ferrous alloys. Maheshwari Brazings offers these alloys in a wide range of compositions to suit specific applications. Available in Wires and Rods, Strips, Wire Flattening, Wire Preforms, Strip Preforms, Granules and Spheres. With the help of the chart below, identify and compare alloys of our Silver Based Cadmium Bearing Alloys suited to your needs.

MBPL RAJAT 67Cd

MBPL RAJAT 67Cd is used for brazing of Silver goods made of silver alloys
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
67 11 12 10 - 635-720
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
- - - -

MBPL RAJAT 50Cd

MBPL RAJAT 50Cd is one of the lowest melting point Silver Brazing alloys available.It has excellent flow characteristics. The highest joint strength can be obtained with this alloy. Has better resistance to corrosion in chlorine, sulphur and steam environments
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
50 15.5 16.5 18 - 620-640
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag301 BAg-1a - AG1

MBPL RAJAT 45Cd

MBPL RAJAT 45Cd has the lowest brazing temperature range of the BAg filler metals.It also flows more freely into narrow clearance capillary joints.Its narrow melting range is suitable for rapid or slow methods of heating.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
45 15 16 24 - 605-620
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag302 BAg-1 BACuAg15 -

MBPL RAJAT 44Cd

MBPL RAJAT 44Cd is low melting filler metal for brazing electrical contacts and molybdenum or copper tungsten electrodes.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
44 27 13 15 1P 595-660
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
- - - -

MBPL RAJAT 43Cd

MBPL RAJAT 43Cd has the shortest melting range of any silver brazing alloys. This alloy is regarded as the best brazing alloy by manu brazers. It is particularly recommended where a minimum brazing temperature is desirable to preserve the properties of the parent metals. Ideal where joints have a close fltup and will produce neat joints with optimum ductility and strength.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
43 16 / 17 20 21 / 20 - 615-620
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag303 - BaCuAg16A AG2

MBPL RAJAT 40Cd

MBPL RAJAT 40Cd is used for brazing
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
40 19 21 20 Mn 2, CO 2 595-630
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag304 - LAg40cd Ag10

MBPL RAJAT 35Cd

MBPL RAJAT 35Cd is a free flowing general purpose brazing alloy.Its broader melting range is helpful where clearances are wide or not uniform. Unless heating is rapid, care must be taken that the lower melting constituents do not separate out by liquation
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
35 26 21 18 - 610-700
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag305 BAg-2 BACuAg-20 Ag-11

MBPL RAJAT 35Cd

MBPL RAJAT 35Cd is a free flowing general purpose brazing alloy.Its broader melting range is helpful where clearances are wide or not uniform. Unless heating is rapid, care must be taken that the lower melting constituents do not separate out by liquation
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
30 27 23 20 - 607-710
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag306 BAg-2a BaCuAg21 Ag21

MBPL RAJAT 251Cd

MBPL RAJAT Silver 251Cd has good fillet forming properties with an ability to bridge wide gaps. The wide melting range limits its applications and it is not normally recommended for applications with slow heating rates.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
25 30 27.5 17.5 - 605-680
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag307 BAg-33 - -

MBPL RAJAT 250Cd

MBPL RAJAT 250Cd has good fillet forming properties with an ability to bridge wide gaps. The wide melting range limits its applications and it is not normally recommended for applications with slow heating rates.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
25 35 26 14 - 605-745
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
- BAg-27 - -

MBPL RAJAT 20Cd

MBPL RAJAT 20Cd has good fillet forming properties with an ability to bridge wide gaps. The wide melting range limits its applications and it is not normally recommended for applications with slow heating rates.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
20 40 25 15 - 605-765
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
Ag309 - - -

MBPL RAJAT 12Cd

MBPL RAJAT 12Cd is an economical alloy with wide melting range. Like above, preferred for applications having short heating cycles to avoid liquation. Ideal for bridging wider gaps where work pieces are insensitive to heat.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
12 50 31 7 - 620-825
Specifications
DIN:8513 AWS:A5.8 IS:1278 BS:1453
L-Ag12Cd - - -

MBPL RAJAT 5Cd

MBPL RAJAT 5Cd is used where alloy having higher melting point and better strength than soft solder is required.
Send Enquiry
Nominal Composition % Melting Range
Ag Cu Zn Cd Others ºC
5 - 7 - - 335-392
Specifications
EN:1044 AWS:A5.8 IS:2927 BS:1845
- - - -